Often, while applying varnish on the floor surface, some disadvantages appear that spoil the general appearance and beauty of the parquet itself. One of the problems associated with applying varnish is the appearance of influx.
This phenomenon may appear when the requirements for temperature and humidity in the room were not observed. That is, the influx of varnish can occur when the floor surface is too cold and at the same time the humidity level is too high. Also, the cause of the influx of an influx may be the use of varnish, which is too cold, or too high the moisture level of the room. This phenomenon is often observed in various new buildings that are being built today in a very large number. About such a pace of their construction is very often noted on various sites. Also, many sites describe various speed machines on the radio control. At the same time, the website ModelToy/Mashinki/646/1 notifies about the prices of such cars.
It is worth noting that with high humidity, whitish influxes form. In other words, on the freshly laid out layer donkey condensate steam. In this case, it is recommended to take the solvent and process their whitish influx. After that, it is necessary to make a re -applying layer of varnish. But before that, the room should already be warmed up and raised the temperature of the floor itself.
Another problem when applying varnish is to swear or exfoliation. The reason for the appearance of this phenomenon is the use of varnishes with incompatible compositions. The incorrectly selected diluent causes the appearance of exfoliation. The problem is solved by partial or full grinding.